Magna-Ject Pink Ferris Bead Wax - 5lbs

SKU
74-0600-JECT
Link Copied to Clipboard
$33.75
  • Brand: Ferris
  • Style: Bead
  • Color: Magna-Ject Pink
  • Application: Very Fluid, low shrinkage and non-brittle
  • Injection Temperature: 70ºC / 158ºF
  • Country of Origin: United States
  • Priced Per: 5lb package
Link Copied to Clipboard
Priced Per 5-lb Package
Qty Price Per Unit
1-2 $33.75
3-9 $33.08
10 and Above $32.40
  • Magna Ject Pink Ferris Bead Wax is an extremely fluid wax for filling the most intricate pieces, including filigree, even at low pressures.
  • It is low shrinkage, durable, and non-brittle with a long shelf life.

 



Injection Wax Trouble Shooting Guide



Problem Remedies
Wax Pattern Sticky-Pattern Distortion - Reduce wax temperatures
- Increase pattern dwell time
Pattern Flashing/Fins Mild Overfills - Reduce wax temperature
- Clean mold vents, increase size & quantity of vents
- Reduce air pressure
- Hold mold firmly/keep locks aligned
- Allow mold to cool
Excessive Pattern Shrinkage - Reduce wax temperature
- Use low shrink/low sink wax
- Use warmer mold
- Increase pattern dwell time
- Increase air pressure
- Increase sprue size
Sink Area on Large or Heavy Patterns - Reduce wax temperature
- Use a low shrink/low sink wax
- Increase pattern dwell time
- Increase air pressure
- Increase sprue size
Air Bubbles in Patten  - Reduce wax temperature
- Increase wax temperature
- Reduce air pressure
- Make sure wax pot is full
- Minimze trapped air in wax
- Fit mold properly & securely onto injection nozzle
No Mold Fill or Partial Mold Fill - Increase wax temperature
- Use warmer mold
- Clean mold vents, increase size & quantity of vents
- Increase air pressure
- Increase spure size
- Reduce mold release spray/do not use talc
- Use a more fluid was to fill thin sections
- Make sure injection nozzle is not clogged
- Do not hold mold too tightly
Ripple on Pattern Surfaces - Increase wax temperature
- Use warmer mold
Cracking/Brittle Wax Patterns - Use a more flexible/ductile wax
- Reduce pattern dwell time
Roughness on Pattern Surface - Use a smoother, more polished master
- Reduce mold release spray/do not use talc

Product SDS

Packing Qty Priced Per 5-lb Package